6 / 7 page ![]() Figure Recommended condition of reflow soldering Recommended peak temperature is over 245 OC. If peak temperature is below 245 OC, you may adjust the following parameters: Time length of peak temperature (longer) Time length of soldering (longer) Thickness of solder paste (thicker) Conditions of hand soldering Temperature: 370 OC Time: 3s max. Times: one time Storage conditions Temperature 5 to 40 OC Humidity 30 to 80% RH Recommended period One year after manufacturing PJM2302NSC N- Enhancement Mode Field Effect Transistor 6 / 7 www.pingjingsemi.com Revision:1.1 Oct-2017 www.pingjingsemi.com Revision:1.1 Oct-2017 Conditions of Soldering and Storage www.pingjingsemi.com Revision:1.0 Jun-2019 50 100 150 200 250 (°C) 0 Pre Heating Rate Reflow Heating Rate Soldering Peak Temperature Cooling 1 to 5°C / s Preliminary Heating 130 to 170°C, 50 to 120s 230°C, 20 to 30s 60s min. 1 to 5°C / s 245 to 260°C, 10s max. 2 times max. |
|
|
Enlace URL |
| ¿ALLDATASHEET es útil para Ud.? [ DONATE ] |
Todo acerca de Alldatasheet | Publicidad | Contáctenos | Política de Privacidad | Enlace a la hoja de datos | Intercambio de Enlaces | Lista de Fabricantes All Rights Reserved©Alldatasheet.com |
| Russian : Alldatasheetru.com | Korean : Alldatasheet.co.kr | Spanish : Alldatasheet.es | French : Alldatasheet.fr | Italian : Alldatasheetit.com Portuguese : Alldatasheetpt.com | Polish : Alldatasheet.pl | Vietnamese : Alldatasheet.vn Indian : Alldatasheet.in | Mexican : Alldatasheet.com.mx | British : Alldatasheet.co.uk | New Zealand : Alldatasheet.co.nz |
|
Family Site : ic2ic.com |
icmetro.com |